Grinding belts and grit progression
Guide · last changed 20 November 2026
Use coarse ceramic belts to remove steel, step through the grits without skipping far, and put on a fresh belt after heat treat. Belts are a consumable: a dull one costs more in heat and time than a new one costs in money.
Belt types
| Type | Use it for | What to know |
|---|---|---|
| Ceramic | Profiling and grinding bevels, 36 to 120 grit | Cuts fast and cool and lasts longest on hardened steel. It needs firm pressure to keep fracturing fresh edges; used lightly, it glazes. |
| Zirconia | Rough work on a budget | Cheaper than ceramic and shorter-lived. Fine for profiling. |
| Aluminum oxide | Handle materials and light finishing | Inexpensive. Dulls quickly on hardened steel. A flexible (J-weight) backing follows curves, which suits handles. |
| Structured abrasive | Refining a blade finish, roughly 120 to 600 grit and finer | Sold under names such as Trizact. Leaves a very even scratch pattern and wears consistently. Use light pressure. |
| Non-woven (surface conditioning) | A satin finish and blending | The same family as abrasive hand pads. Evens out a finish without removing much steel. |
| Cork or felt with compound | Polishing | Optional. Used for a bright finish after the fine grits. |
A progression that works
Before heat treat
- 36 or 60 grit ceramic: profile the blank and grind the bevels most of the way. Leave the edge about 0.8 mm (1/32 in, about the thickness of a credit card) before heat treat; thinner edges warp and crack more easily.
- 120 grit: remove the coarse scratches and true up the grind lines.
- 220 grit: a clean surface to go into heat treat. Deep scratches left now are hard to remove from hardened steel.
After heat treat
- A fresh 60 or 120 grit ceramic belt: grind off the scale and bring the edge down to its final thickness. Use a fresh belt, light passes and bare fingers on the blade, and dip it in water often. The thin edge heats much faster than the part under your fingers, so cool it before it feels hot.
- 220, then 400: with ordinary belts, or the equivalent structured belts.
- Stop on the grinder at 400 to 600 for a belt finish, or go to a non-woven belt for satin.
Hand sanding
For a hand-rubbed finish, wrap wet/dry sandpaper around a hard, flat backer and sand lengthwise with a little oil or soapy water. Start one step coarser than your last belt, and change direction slightly with each grit so you can see when the previous scratches are gone. 400 or 600 grit is a practical working finish; higher grits look finer and show every mark.
Grit equivalents for structured belts
Structured belts are graded by particle size in microns, with an A prefix; a lower number is finer. Published conversion charts do not agree exactly, so treat these as approximate.
| Grade | Roughly equal to |
|---|---|
| A300 | 80 grit |
| A160 | 120 grit |
| A100 | 180 to 220 grit |
| A65 | 240 to 280 grit |
| A45 | 320 to 400 grit |
| A30 | 400 to 800 grit, depending on the chart |
Habits that save belts and blades
- Do not jump too far between grits. Roughly doubling the grit at each step works. Going from 60 straight to 400 leaves coarse scratches that the fine belt will never remove.
- Retire dull belts from blade work. A dull belt rubs instead of cutting and overheats the edge. Keep worn belts for handle shaping and deburring.
- Keep steel belts and handle belts separate. Steel grit embedded in a belt will stain light-colored wood and bone.
- Slow down for handles. If your grinder has variable speed, use a low speed on wood and synthetics, which scorch and clog belts quickly.
- Wear a respirator. Grinding dust, and especially dust from handle materials, should not be breathed.
Long blades, fullers and spearheads
- The same progression, in longer passes. Work a sword blade in full-length passes from guard to point at an even speed, and count passes per side. Stopping part-way leaves a dip that shows down the whole blade.
- Flat platen or a long hard backing for the flats. A slack belt rounds a long bevel. For hand sanding use a hard, flat block at least 150 mm (6 in) long and sand lengthwise.
- Fullers. Rough the groove with a small contact wheel or a round-faced wheel run along a fence, then clean it with paper wrapped round a dowel or a shaped hard block, lengthwise only, through the same grits as the rest of the blade.
- Budget more belts. A sword has many times the surface of a knife. Coarse ceramic belts do most of the work; have several fresh ones before you start.
- Keep it cool after heat treat. A thin tip on a long blade overheats fast. Dip often and use light pressure toward the point.
- Spearheads grind like a double-edged dagger: four bevels meeting on a center ridge. Mark the ridge on both faces and grind all four evenly; the inside of a socket is cleaned with paper on a dowel.
For a sword or a spear, see making a sword or a spear.
Belt sizes
Buy belts for the machine you have: 1×30 and 2×42 for small benchtop sanders, 2×48 and 2×72 for dedicated knife grinders. The 2×72 size has by far the widest choice of abrasives, which is one reason it is the standard for knife making.
Where to buy
- Red Label Abrasives: grinding belts and knife-maker belt kits.
- Combat Abrasives: grinding and finishing belts.
- Pops Knife Supply: belts alongside steel and handle material.
BLANKSMITH is not paid for these links today; some may earn a commission in the future. See the disclosure.
See the belts your design needs
BLANKSMITH's shopping list includes the abrasives for the knife you designed, with a grind set-up sheet for the bevels.